Jay Fisher - Fine Custom Knives

New to the website? Start Here
"Vindicator" push dagger, obverse side view in CPM154CM powder metal technology tool steel blade, 304 stainless steel bolsters, Afghanistan Lapis Lazuli gemstone handle, hand-carved leather sheath inlaid with Elephant skin
"Vindicator" with Lapis Lazuli Gemstone handle

ATS-34: Beyond Chrome/Moly Tough

"Ari B'Lilah" professional counterterrorism knife, obverse side view in ATS-34 high molybdenum alloy stainless steel blade, T3 advanced cryogenic treatment, 304 stainless steel bolsters, ghost slate finish, G10 fiberglass/epoxy composite handle, hybrid tension-locking sheath in kydex, anodized aluminum, 304 stainless steel, titanium
Ghost Slate finish, Shadow Line Counterterrorism Knife "Ari B'Lilah"in ATS-34
"Corvus" chef's knife, reverse side view in ATS-34 high molybdenum alloy stainless steel blade, 304 stainless steel bolsters, Pietersite gemstone handle
"Corvus" Chef's Knife in thin, hard, and tough mirror polished ATS-34 high molybdenum martensitic stainless steel


"Ghroth" professional counterterrorism, combat, tactical knife, obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, coyote/black/olive G10 fiberglass/epoxy laminate composite handle, locking kydex, anodized aluminum, stainless steel, titanium sheath
"Ghroth" Counterterrorism/Tactical Combat Knife in Shadow Line Black ATS-34
"Ananke" fine custom handmade knife, obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Kambaba Jasper gemstone handle, hand-carved leather sheath inlaid with buffalo skin
"Ananke" Khukri in ATS-34 high molybdenum martensitic stainless steel blade

What is ATS-34?

A martensitic stainless steel. It's composed of these major alloy elements (I don't list the minor elements since they don't play a major role) :

  • Carbon: 1.00% - 1.25% This increases hardenability and wear resistance, but decreases toughness in higher amounts.
  • Manganese: 0.40% This is added to reduce brittleness and improve forgeability, hardenability, and reducing deformation.
  • Silicon: 0.25% This is a deoxidizer and improves hot-forming properties.
  • Chromium: 13.75% -14.00% Added only to high alloy tool steels, this improves hardenability, high wear resistance, toughness, and corrosion resistance.
  • Molybdenum: 3.5% - 4.0% Improves deep hardening and toughness, while adding hard and wear-resistant molybdenum carbides (when properly cryogenically processed).

These basic elements (along with iron) are a simple combination that works well together, and has for decades.

More than Chrome/Moly?

There is a distinctive steel class, loosely identified as Chrome/Moly. This steel has a reputation for extreme toughness and durability with elevated hardness. These steels are in the 41XX SAE grade, and are used in race car and bicycle frames, aircraft tubing and even rifle barrels. But even these great steels pale in comparison to ATS-34. While 41XX series steels contain some chromium, it is not even close to the amount in ATS-34. The same can be said for the carbon and also the molybdenum. While the reputation for the chrome/moly steels is well deserved, ATS-34 could be described as chrome/moly evolved and refined to tool grade status, or chrome/moly on super-steroids. Here's a chart that illustrates this.

Critical Alloy comparison between Chrome/Moly and ATS-34 Steels (in percent)
Steel Type Carbon Chromium Molybdenum
Chrome/Moly (4130) 0.3 1 0.2
ATS-34 1.25 14 4.0
Percentage Difference +417 +1400 +2000

I left out the less critical alloys to illustrate the profound differences in these steels. While the two steels both have elevated levels of chromium and molybdenum, they are totally in separate genres. The reason I made this comparison is because it's easier to see those differences to give the layman a more generalized understanding of the superiority of tool grade stainless steels and more commonly known and respected chrome/moly steels. Pretty impressive, I think!

For more information, link to my Heat Treating and Cryogenic Treatment of Knife Blades page.

Back to page topics

"Imamu" obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, tiger stripe G10 fiberglass/epoxy composite handle, locking kydex, aluminum, stainless steel sheath with ultimate belt loop extender, diamond sharpener, firesteel/magnesium fire starter, HULA flashlight holder with XL series Maglite
The incredible toughness and durability of high alloy ATS-34 tool steel on this Imamu
"Zeta" fine handmade custom knife in T3 cryogenically treated ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Indian Green Moss Agate gemstone handle, hand-carved leather sheath inlaid with green rayskin
The clean lines and mirror polished beauty of ATS-34 in this "Zeta"

ATS-34: Super Durable, Super Tough

Some history: From my research and experience, ATS-34 is a Japanese version of 154CM, a high chromium, high molybdenum stainless tool steel. The company actually lists this metal as ATS34 (without the dash). It's hard to find an actual reference detailing the origin of both of these steels. Like most knifemakers, I heard through anecdotal details that 154CM (and ATS-34) was developed for jet engine turbine blades, but I can't find a verifiable source for this. 154CM had been around a while when I started making knives, and it's not an actual steel designation, but a trade name.

Why do I mention 154CM? That's because, in nearly every respect 154CM and ATS-34 are the same steel; they have the same alloy contents in virtually the same amounts. A problem arose in the 1980s, when guys like Bob Loveless were using 154CM and touting its wonderful properties; steel mills in the U.S. making the stuff were evidently dropping their quality controls. There was a lot of movement in the steel industry at the time, and mills were closing all over the country. Whatever the reason, we American knifemakers started finding pits, voids, inclusions, and spots in these 154CM steel bars. A knifemaker cannot tolerate the slightest pinhole in a blade, even if he didn't pour the steel and it's not his fault; a knife with a hole or dark spot on the stainless steel blade just won't sell. So knifemakers in those days talked about 154CM and how bad it was getting, when we found out that the Japanese were making ATS-34, their version of this great steel, and the bars and stock were much cleaner, with no voids, holes, inclusions, or debris in the billets. We all heard stories of their quality controls, double pouring, in vacuum furnaces, and high purity environments. So in the 1980s, most of the makers moved to ATS-34. I've read a lot of confusing stories about this movement and direction of steel sources on the internet, and there is a lot of confusing misinformation about the origin of both of these steels. No matter; this is how it played out for me (and a lot of other knifemakers) in the 1980s. We found spots, holes, and inclusions in 154CM blades, could not sell them, and moved to ATS-34 because it was cleaner. Technically, they are the same steel, with only very minor differences in alloy content.

Post-1980s: 154CM made a reappearance, mainly by Crucible Industries. In 2006, they developed CPM154CM, a particle metallurgy tool steel, made by the powder fusing process. This is a fantastic steel, deserving of its own recognition, but it is not the 154CM of the past that was poured in traditional method. The difference is simply the CPM (Crucible Particle Metallurgy) designation. This designation means the steel was sprayed (particles) into a non-segregated mass and pressure forged. More on CPM154CM on its own page.

Late 2019: ATS-34 is a tremendous stainless tool steel, and unfortunately, it's not being imported much anymore because its just too expensive! Our American suppliers aren't able to afford it anymore, so it's harder and harder to get. I still use it on some of my best knives, when extreme toughness along with high hardness and wear resistance is required. If you wonder why this great steel isn't being used on chef's knives from Japan instead of colored wrapper stuff, just remember that it's an expensive, high alloy stainless steel that requires costly processing.

ATS-34 is a fantastic steel, and because it's been around a while, it's not as intriguing as the newest, latest, pop steel alloy. Do not sell this steel short; it is one of the finest knife blade steels made, with some great properties that are unique and valuable. A very simplified way to understand this steel is to compare it with 440C (featured on this page). You might consider that these steels are essentially the same, except 3-4 percentage points of chromium have been replaced by molybdenum. That pretty much sums up the difference. What this yields is a tool steel that has somewhat less corrosion resistance than 440C, and reduced chromium carbides, but has markedly greater toughness, with additional molybdenum carbides for high wear resistance. Toughness is key here; it's resistance to breakage or fracture, and this is important to consider in very thin blades that will be under high lateral stress, impact, or are of great length where toughness is key to reduce the possibility of fracture. The chart below will help define this relationship.

To understand this balance between chromium and molybdenum, see this simplified table:

Wear Resistance and Toughness in Chromium Steels
Alloy Amount Alloy Content Beneficial Effect Limitation
⇑ Chromium High Chromium, Low Molybdenum Higher corrosion resistance Lower toughness
Balance Chromium and Molybdenum in balance Balanced for particular use Good combination of corrosion resistance and toughness
⇑ Molybdenum High Molybdenum, Low Chromium Higher toughness Lower corrosion resistance

Note that in this chart, unlike the chart on the page dedicated to 440C, carbon has been left out of this comparison. I did this because the carbon content in both 440C and ATS-34 is about the same. The difference in these two steels is the chromium-molybdenum balance. ATS-34 sacrifices the benefits of chromium (mainly higher corrosion resistance) to add molybdenum, which gives it a markedly greater toughness.

Another factor in ATS-34 is that it is a Food Contact Safe steel, but only if properly heat treated. What is the proper heat treatment? It absolutely requires a deep cryogenic processing to bring out the superior nature of this steel, including corrosion resistance. That is why the treatment must adhere to the Standard NSF § 7.1,

The choice of 440C vs. ATS-34 then becomes one of exposure and use, along with availabiltiy. For instance, in my professional tactical combat knives, if marine and jungle environments are to be expected, 440C is usually chosen because it is simply more corrosion resistant than ATS-34. If extreme use and toughness is expected, ATS-34 is chosen. It also depends on the knife geometry and grind. If very thin areas exist on the blade, components, or features, ATS-34 may be a better choice; it's less likely to break under severe mechanical stress in thin cross-sectional areas simply because it's tougher.

ATS-34 is very tough.

Back to page topics

"Charax" dagger in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Australian Black Jade, California Jade gemstone handle, stingray skin inlaid in hand-carved leather sheath
Elegant and tough, the fuller-ground Charax dagger with mirror polished ATS-34 blade
"Krag" professional tactical/counterterrorism knife, obverse side view in ATS-34 high molybdenum stainless steel blade, ghost slate finish, 304 stainless steel bolsters, black/red G10 handle, hybrid tension locking sheath in kydex, anodized aluminum, stainless steel, titanium
ATS-34, Shadow line in Ghost Slate on this "Krag" Counterterrorism, Tactical Combat Knife

High Heat Resistance

ATS-34 steel is that it can be processed to have very high heat resistance, at the expense of toughness and corrosion resistance. This steel can be  tempered at or above 1000°F (538°C), into the secondary hardening range. This steel is much more wear-resistant and harder when tempered at the higher range. It is also stiffer. This would be represented in the yield strength, which, in my processing experience, is higher at a higher temperature tempering process, with this particular steel in this narrow application. So there is a totally different character in this steel depending on how it's processed.

If a steel blade is to encounter extremely high temperatures, the higher tempering range (secondary hardening range) would be the way to go, but it will sacrifice tremendous corrosion resistance and toughness. When tempered at the higher range, in order to affect a change the actual hardness, toughness, and temper of the blade, the blade steel in use would have to be heated to above 1000°F. This is very hot, and it's extremely unlikely that the steel would encounter that temperature during most uses. So, even short exposure to a fire won't change the temper of this steel if tempered in the higher ranges. Also, when sharpening, motor-driven sharpening tools (wheels, buffs, abrasive) would have to bring the edge up to above this temperature to affect the temper.

Just like any balance of characteristics, there are also costs. Tempering this steel in the secondary range is not recommended if a blade is thin, or if it's expected to have substantial corrosion resistance. Rarely is this done and it's not recommended on knives, but in special applications. There are other technical problems with tempering in the secondary range like grain coarsening and instability, so it's not typically done. However, I've had a few custom knives where a client has requested this, so it's not completely off the table.

Back to page topics

"Horus" obverse side view in ATS-34 high molydenum stainless steel blade, 304 stainless steel bolsters, engraved, Micarta phenolic handle, locking kydex, aluminum, stainless steel sheath with black lacquered brass engraved flashplate.
Military combat grade tough ATS-34 blade of this Horus
"Hooded Warrior" obverse side view in ATS-34 high molybdenum stainless steel blade, hand-engraved 304 stainless steel bolsters, Australian Tiger Iron gemstone handle, locking kydex, aluminum, stainless steel sheath
"Hooded Warrior" tactical knife with mirror polished ATS-34 blade

Polish and Finish

The inclusion of chromium at more than 12% means ATS-34 is a true stainless steel. ATS-34 polishes and finishes beautifully. While there is always a grain visible in the metal, it is comparable in appearance to 440C. The grain may have interesting patterns and flow banding when polished, which does not effect the value or performance of the knife. A bit of orange peel granularity can sometimes be seen, though it is lighter and less distinctive than that found in polished D2.

A high polish in ATS-34 improves its corrosion resistance overall. Unlike many of the more wear-resistant knife steels, ATS-34 holds the high finish indefinitely with little care. In fine art pieces, ATS-34 can be engraved, and the imagery stands out well against a mirror polished blade. Like most of the finer cutlery steels, ATS-34 can be difficult for the knifemaker to polish, taking many steps to achieve a brilliant luster, but it's worth the effort. It's also ridiculously hard to engrave, and most engravers won't touch it. I do, and I like the results.

Back to page topics

"Manaya" hatchet sculpture in hand-engraved ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Nephrite Jade, Green Goldstone gemstone handle, stand of Walnut, Oak, Tulipwood, Jade, Migmatite Granite
Hand-engraved ATS-34 stainless steel blade in this Manaya
"Skeg" tactical, counterterrorism professional knife in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, ghost slate surface treatment, handle of carbon fiber, hybrid tension-lock sheath in kydex, anodized aluminum, stainless steel, titanium
"Skeg" Tactical Combat/Counterterrorism Knife in ATS-34, Ghost Slate Finish

What about the newer alloys?

Like 440C, ATS-34 has been around a while. It's not a new, exciting, or proprietary steel, it's not a gimmick, not a flash in the pan. It's been around a while strictly because it is a very good steel; it has staying power. The same thing can be said of D2, the extremely high carbon die steel, and 440C, the martensitic stainless steels that all others are usually compared to. These (and many others) are not new steels, and thus, they are not as pop-exciting as some of the newer alloys.

Are there other good alloys? Of course there are, and some of them have marked advantages over ATS-34. You may be surprised to hear that at the time of this writing, I use over a dozen different steels, and every one of them has certain advantages and certain (and sometimes defeating) limitations. Take the CPM steels, made by the crucible particle technology process. They are great steels, they are very expensive, and each one has its own attributes. CPM154CM is a beautiful steel, but when compared to ATS-34, is much more expensive and limited in available sizes. CPMS35VN is tougher, but it can't be mirror polished, has a lower tempering temperature, is very expensive, and limited in available sizes. You won't see this on their data sheets.

By the way, don't always trust manufacturer's data sheets, Crucible Steel reps have told me face to face that there are "misprints" on these sheets. One such misprint is claiming that CPMS35VN can be mirror polished, but, in truth, it can't be mirror polished due to the high vanadium carbides that are present after heat treating. Whoops! Okay, it's "just a misprint." So if you can't entirely trust a manufacturer's data sheet, what can you trust? Who you should be able to trust is someone who has had decades of using many steel types for many knives; they are the guys with the know-how. More on that below.

Another example of painting newer steels as superior can be found in what is not said. Many of these newer alloys have totally ignored finishing as a benefit. Finishing is the ability for a knife blade to be polished to a high, even mirror-like finish. This is critical in art pieces and investment grade knives, and also critical to keep the highest corrosion resistance possible. A rough blade corrodes easier, simply because of increased surface area. More on that topic here.

There simply is no ultimate steel for knife blades, no superior, magnificent, ultimate blade material. Each choice of steel for a knife blade is a decision of balance of many properties.

Knife buyers are just like everybody else; they can be swayed towards a particular knife buying decision based on advertising. Who wouldn't want the newest truck, the newest tool, the newest snack, or the newest knife? How do you make a knife, a tool that has existed for longer than any other tool in the history of man sound and seem new? Sure, people need knives, they use knives, and they collect knives. What could be more appealing than the newest, most exotic, most astounding performing steel made today? Why, even I would want to buy that! One problem though: it doesn't exist. See the next topic.

Back to page topics

"Kotori" in ATS-34 high molybdenum stainless steel blade, hand-engraveds 304 stainless steel bolsters, Carnival Lace Agate gemstone handle, hand-carved, hand-dyed leather sheath
The tough, radical double hollow grinds on this ATS-34 blade of Kotori
"Hooded Warrior" obverse side view: fine custom tactical, combat knife in ATS-34 stainless steel, 304 stainless steel bolsters, Black Palm Wood hardwood handle, locking kydex, aluminum, stainless steel sheath
"Hooded Warrior" has one of the toughest, most versatile blades of ATS-34

Why do they claim their steel is superior and how can I find the truth?

There simply is no ultimate steel for knife blades: no superior, magnificent, ultimate blade material. Please understand this: If there were a steel superior to all other exotic metals, all others would be cast aside, no longer made at any foundry, and they would be sentenced to the ashbin of obsolescence. Every steel has its pros and cons, its advantages and disadvantages. So advertisers need to make something sound new and better (even if it is cheaper and worse), so they claim a new steel, a better steel, a rarer steel, a superior steel is used in their product. Isn't it funny that they never claim new or superior handles, bolsters, or sheaths, only the blade steel! That's because they know that you, as a consumer, have limitations that prevent you from knowing the truth. How does this happen?

  • They know that you will not have the steel tested by a certified metallurgist to determine exactly what the steel is.
  • They know that you will not use the knife in such a way as to notice any difference in any performance from earlier steels.
  • They know that there is no real testing of knife blade steel performance, only subjective comparisons based on vague properties that are not scientifically defined.
  • They know that if you are unsatisfied, they amount you pay is either not enough for you to care about, is not too much for them to refund, or that you will be satisfied with a replacement of the same item.
  • They know that you are influenced, hoodwinked, and taken in by advertising hype consisting of unsubstantiated claims.
  • They know that there is no official, law enforcing, or sanctioned authority that will police their lies, claims, and inflated hype to make them tell the truth in their advertising.
  • They think you are too stupid, ignorant, or careless to bother to research the topics presented by proven masters and highly experienced professionals in this field, and will simply go with the herd.
  • They know you, who are reading this website, are not their customers.

Okay, so is most of what you read about knife blade performance hype? It really depends on who is presenting it, and this is very important. If you are a knife client, buyer, or user, there is a simple way to know whether your knifemaker, knife factory, and knife supplier is selling the hype or knows what he is talking about. Look at his knives!

  • Look at the website; if there isn't a substantial web presence, they are not modern or advanced makers tuned to make and respond to modern knife use, design, or appeal. Their website demonstrates their participation, or lack thereof, in the professional knifemaking field. Look for information, lots of it. There simply is no reason a knifemaker or (worse) a knife manufacturer will not take the time to offer every available piece of information about the product they sell. If I, as an individual knifemaker can do it, certainly a large corporation with dozens or hundreds of employees can too! If it's a single knifemaker you intend to buy from, know that how he "wears" his website demonstrates how he treats his clients, because this is the service aspect of our field. More on service at this bookmark.
  • Look at his testimonials. Are they realistic, are they plentiful? Do they seem like they are all made by one writer, or do the individual testimonials have their own voice?
  • Look who he makes for. This should be clearly presented, with plenty of references, testimonials, and types of knife in his particular field.
  • Look at his history. A new maker is not an experienced maker. There is no shortcut, no fast track to knifemaking skill. There is no cultural claim to fine knives (like is so often seen in Japanese style sites and products). The history of the maker should be well established and clearly defined without hype.
  • Overall and most importantly: LOOK AT THE KNIVES! Do they look finely made, are the grinds crisp and uniform, are the finishes complete and precise? Do they have an excellent and precise fit? Do they even offer large, clear, and plentiful photos that you can see the fit at all, or are they just small, dinky "profile" photos? Have they painted the blade? Are there three ridiculous rivets securing the handle to the tang? Is the tang tapered for balance? Are the blades ground to their purpose, are there a large variety of styles, patterns, and designs to choose from, or are they just 4" drop points? Are the handle materials wide-ranging and exotic, as well as domestic? Are there fittings on the knife (bolsters)? Are there good sheaths? Good stands, good cases? Or is the maker or manufacturer just making a simple, plain, boring knife, and then hyping the steel type in hopes you'll buy?
  • Probably most important: does the maker make real combat knives? Why do I mention this? This is included because real combat knives are frequently the most durable, most well-made, most challenging, and most important endorsements of the maker's experience. I don't mean knives that are stylistically tactical, I mean real combat knives made for and used by professionals in the field of war, counterterrorism, or law enforcement. While many makers and manufacturers claim to be making these knives, their reputation, their illustration and their participation in this field is less tangible and more inferred.
    How do you know the difference between a maker or manufacturer who actually makes real combat knives and the company that just makes the claim? Hold on to your hat: it's the sheath. If a maker or company is making an actual combat knife, the sheath is just as important as the knife, and made just as durable, with specific and various options, with real mounting and interfacing hardware to work with the professional's gear. How do I know this? Because this is how every knife makes it into battle: in a sheath. So don't forget to look over what is (or what is not) offered in this critical part of the knife package; it will tell you a lot!

Most knifemakers and manufacturers who overly hype their steel type produce an inferior product.

Back to page topics

"Arctica" obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, red/black G10 fiberglass epoxy composite handle, locking kydex, aluminum, stainless steel sheath with full accessory package
The incredibly tough and durable blade and military combat sheath and accessories of this "Arctica"
"Corvus," obverse side view in ATS-34 high molybdenum martensitic stainless steel blade, T3 Cryogenically treated, 304 stainless steel bolsters, Majestic Agate gemstone handle, silicone prise
"Corvus" Chef's Knife with incredibly thin, hard and keen hollow ground ATS-34

Why don't you see more ATS-34 blades?

ATS-34 is a long regarded, well-applied tool steel, and it has many applications in the industrial and military field. Just as with 440C, ATS-34 is not a new star, a rising gimmick, or a catchy pop steel. It is a very tough steel, reliable, finishes well, and wears durably in the fields of combat and utility, while having the beauty to take its place in the collector's sculptural knife world. Many of the best knifemakers in the world use or have used this fine steel. So why don't you see it more often used?

  • It's not a new steel, therefore does not gain pop attention.
  • It's difficult to work with, requiring processing in a clean and specific controlled environment.
  • It is not a steel that can be hand-forged. It requires a high purity environment, and very high forging temperatures, and clean atmosphere during heat treatment.
  • The best processing of ATS-34 is in deep cryogenics. While it can be processed in conventional treatment, this will not yield the very best allotrope and fine eta-carbide structure, only deep cryogenics will.
  • The temperatures during the processing of this steel are critical; a very accurate oven/pyrometer/control system is vital, frequently tested and calibrated for certainty.
  • It is difficult to polish and finish, requiring many steps of abrasives to bring to a bright finish.
  • It is not forgiving. Once it's been hardened and tempered, there is no correction, no "fixing" any mistakes.
  • It is a more expensive than standard carbon steels, and a bit more expensive than 440C.

Processing Controls: Just as with 440C, this steel can be badly handled during the essential stages of making a knife blade, and any errors here can result in a botched result. This usually shows as a knife that is more brittle than acceptable or more soft than intended for use. While many of the new makers are sending high alloy martensitic stainless steels out to be processed, who is assuring that the absolute critical and distinctive controls of the process are being accomplished?

I know of one instance where a maker found out that his ATS-34 blades were being processed in a batch of 440C blades. This was done because the heat treater simply did not have enough of the ATS-34 blades to fill out his batch, so he just stuck the two types together, and processed for the 440C. This is essential to understand: these steels do not process the same, ATS-34 has a distinctively higher critical temperature, and different quenching process than 440C. So the performance of the ATS-34 was markedly degraded. My own experience has determined that an interrupted fast quench yields a much higher initial hardness on this steel; the same process on 440C would ruin it. Additionally, the higher tempering set is not something most makers (and heat treaters) are doing, and has to be considered for each individual knife blade and application. This is not just my opinion; I've discussed this with engineers and suppliers of this steel and they all have the same opinion: ATS-34 is a fantastic steel when processed correctly. More about this on my Heat Treating and Cryogenic Processing of Knife Blade Steels page.

Finish value is rarely discussed by novice or unskilled or non-professional knife makers and is never discussed by any factory, because many makers (and all manufacturers) never, ever finish a blade, simply settling for sanding to 320 grit like a piece of pine in a weekend hobby project. Manufacturers don't finish anything; they mass process with automated machinery and then get the product out the door. Since ATS-34 has less chromium than many other steels, a high finish is critical for a knife that is not combat grade or non-reflective. It takes a lot of time, patience, effort, and skill to properly mirror polish any blade, but that is how all of the finest investment grade knives reach their zenith. You'll see a lot of guys justifying why they don't mirror polish, and most of it is lack of skill and patience.

The reason some of my ATS-34 blades are not mirror polished is simple:

  • The client requests a flat finish because he does not want reflectivity (usually military or combat knives)
  • The client can't afford the extra expense of a mirror polish.

You'll see that the collaborative works on this website with new makers who do not have the skill level yet to attain a mirror polish and appropriately. Practice, skill, and patience build in this field and I'm confident that these new makers will attain this highest of desired finishes, but MOST other makers in the world do not bother. They simply choose not to mirror finish. When making this choice, they have no real standing or experience in evaluating or judging a steel like ATS-34 on corrosion resistance particularly since it has less chromium.

Back to page topics

Note! (to knifemakers)

I've noticed that this page gets a lot of attention from knifemakers, and discussion goes on and on about this steel, how to heat treat it and what to expect. This can get out of hand, with guys claiming to know special bonding structures of the grain, grain size and shape, and describing various methods to achieve certain invisible, unproven, and ridiculous results. Here's my take on this:

Heat treat each piece of ATS-34 according to the manufacturer's directions. THAT'S IT! You don't have to try to better their process; the foundry knows how they made the steel and they politely and effectively tell you how to heat treat it for the best performance.

Why?

All ATS-34 is not the same! Since minor variations in the alloy content are certain to occur as a result of foundry process, as a knifemaker this is not your concern. Just heat treat the steel according to the manufacturer's directions.

Good grief, it's easier than baking a cake! When you bake a cake, you have to measure and mix the ingredients, and the foundry has already done this for you!

If, as a maker, you think that you have some better process than the steel supplier, please do tell them your discovery, maybe you can become a metallurgist or engineer. Also be sure to tell every machine shop and industrial manufacturer of machine tools, dies, valves, shears, forms, presses, and every other industry that uses ATS-34. Wait. Do you suppose that these professional industries already know how to achieve the best performance in their steels? Then, who do they get their heat treating information from? Could it be the supplier of the steel? Ahem.

Just follow the steel supplier's directions.

I don't know how this could be simpler. And then spend some time on Fit, Finish, Balance, Design, Accessories, and Service, as these are the real limitations for most knifemakers today.


"Aldebaran" Fine investment grade collectors or using knife, obverse side view: ATS-34 stainless steel blade, 304 stainless steel bolsters, gemstone handle, alligator inlaid leather sheath
The tough, corrosion resistant and beautiful mirror polished ATS-34 blade of this Aldebaran
"Domovoi", obverse side view in ATS-34 high molybdenum stainless steel blade, hand-engraved 304 stainless steeel bolsters, African dumortierite gemstone handle, hand-carved, tooled, hand-dyed leather sheath
The graceful, thin, sharp, mirror polished ATS-34 blade of this Domovoi

The Mimics

There are people in this field who simply mimic what they have heard. I've seen this for decades in this career field. This site and the book I'm writing are my attempt to clarify what has been misrepresented as fact by the uneducated or inexperienced.

It happens too often that knife makers and enthusiasts simply repeat what they have heard or read in some vague advertising hype as fact, without ever doing any research. I've even seen guys pretending to be testers and evaluators of knives and performance making ignorant claims as if they are some authority. By the way, there is NO certified, regulated, sanctioned, or official testing authority of ANY knife performance, process, or construction, anywhere on this earth! This is not strange or unusual, there are many fields of manufactured items that this does not exist, like jewelry, screwdrivers, headstones, or bronze sculptures.

Most of these guys just want free knives and to make a name for themselves; knife groupies, they are. And if a maker refuses to give them a free (and expensive) knife for testing, I've seen them go on rants about the maker and his knives like crybabies teased by a rattle they can't have. If they really want a knife, why not buy one, like everyone else who wants one? It's because they only want it if it's free. How much dedication is that?

The mimics are often people who publicly post their misinformation. My own website, words, and practices of knifemaking have been challenged on plenty on forums, bulletin boards, and through other social conversation means. I expect this; I'm successful, and this is the price you pay for working hard and achieving something. So the mimics will continue to spew their ignorance, based on lack of experience, as most are too lazy to do any actual research, testing, or quality knifemaking on their own.

Thankfully, I have many, many dedicated clients who do their own testing and use in the field, and these are actual trials of these critical tools in combat, rescues, working, and use. They swear by this steel, and often go on to buy more. They have real skin in the game, their own money, and this speaks more than any other type of evaluation. They have given me the freedom and resources to continue this wonderful journey, and I am eternally grateful for their business, dedication, and support!

Back to page topics

"Grim Reaper" obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Petrified Palm Wood gemstone handle, kydex, aluminum, nickel plated steel sheath, Python skin inlaid in hand-carved leather sheath
Tough hollow ground double-edged point of this mirror polished "Grim Reaper" push dagger
"Guardian" Custom Counterterrorism Push/Punch Dagger, obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, G10 composite handle, hybrid tension-locking sheath in kydex, anodized aluminum, anodized titanium, blackened stainless steel
"Guardian" Tactical Push/Punch Dagger in ATS-34

ATS-34 is a tough competitor

ATS-34 has been around a while, and will continue to be a top choice in knife performance. It has some very distinctive traits: high toughness, good corrosion resistance, high polish potential, and high temperature resistance that are not quite matched by other knife blade steels. This, coupled with a good array of available sizes and thicknesses, moderate pricing, and the steel's beautiful and flaw-free uniformity will make certain that this steel will always be valued by combat and working knife professionals and high art collectors.

In knives, there are only a few steels that can compare with its tough beauty while exhibiting the high wear resistance and high temperature resistance. I consider it one of my most dependable, reliable, and durable performers, and that is why it will continue to hold its own in my professional studio.

For more information, link to my Heat Treating and Cryogenic Treatment of Knife Blades page.

Back to page topics

"Cygnus-Horrocks" obverse side view in ATS-34 high molybdenum stainless steel blade, 304 stainless steel bolsters, Crazy Lace Agate gemstone handle, ostrich leg skin inlaid in hand-carved leather sheath
The tough elegance of ATS-34 high molybdenum-chromium martensitic stainless steel on this "Cygnus-Horrocks"

To the Blades page


XHTML 1.0 Validated, Compliant, Link Checked, and CSS Level 2.1 Validated through W3C, the World Wide Web Consortium
Main Purchase Tactical Specific Types Technical More
Home Page Where's My Knife, Jay? Current Tactical Knives for Sale The Awe of the Blade Knife Patterns My Photography
Website Overview Current Knives for Sale Tactical, Combat Knife Portal Museum Pieces Knife Pattern Alphabetic List Photographic Services
My Mission My Knife Prices All Tactical, Combat Knives Investment, Collector's Knives Copyright and Knives Photographic Images
The Finest Knives and You How To Order Counterterrorism Knives Daggers Knife Anatomy  
Featured Knives: Page One Purchase Finished Knives  Professional, Military Commemoratives Swords Custom Knives  
Featured Knives: Page Two Order Custom Knives USAF Pararescue Knives Folding Knives Modern Knifemaking Technology My Writing
Featured Knives: Page Three Knife Sales Policy USAF Pararescue "PJ- Light" Chef's Knives Factory vs. Handmade Knives First Novel
Featured Knives: Older/Early Bank Transfers  27th Air Force Special Operations  Food Safety, Kitchen, Chef's Knives Six Distinctions of Fine Knives Second Novel
Email Jay Fisher Custom Knife Design Fee Khukris: Combat, Survival, Art Hunting Knives Knife Styles Knife Book
Contact, Locate Jay Fisher Delivery Times Serrations Working Knives Jay's Internet Stats  
FAQs My Shipping Method Grip Styles, Hand Sizing Khukris The 3000th Term Videos
Current, Recent Works, Events Business of Knifemaking Concealed Carry and Knives Skeletonized Knives Best Knife Information and Learning About Knives  
Client's News and Info   Military Knife Care Serrations Cities of the Knife Links
Who Is Jay Fisher?   The Best Combat Locking Sheath Knife Sheaths Knife Maker's Marks  
Testimonials, Letters and Emails     Knife Stands and Cases How to Care for Custom Knives Site Table of Contents
Top 22 Reasons to Buy   Tactical Knife Sheath Accessories Handles, Bolsters, Guards Knife Making Instruction  
My Knifemaking History   Loops, Plates, Straps Knife Handles: Gemstone Larger Monitors and Knife Photos  
What I Do And Don't Do    Belt Loop Extenders-UBLX, EXBLX Gemstone Alphabetic List New Materials  
CD ROM Archive   Independent Lamp Accessory-LIMA Knife Handles: Woods Knife Shop/Studio, Page 1  
Publications, Publicity   Universal Main Lamp Holder-HULA Knife Handles: Horn, Bone, Ivory Knife Shop/Studio, Page 2  
My Curriculum Vitae   Sternum Harness Knife Handles: Manmade Materials    
Funny Letters and Emails, Pg. 1 Blades and Steels Sharpeners, Lanyards Knife Embellishment     
Funny Letters and Emails, Pg. 2 Blades Bags, Cases, Duffles, Gear    
Funny Letters and Emails, Pg. 3 Knife Blade Testing Modular Sheath Systems  
Funny Letters and Emails, Pg. 4 440C: A Love/Hate Affair PSD Principle Security Detail Sheaths      
Funny Letters and Emails, Pg. 5 ATS-34: Chrome/Moly Tough
Funny Letters and Emails, Pg. 6 D2: Wear Resistance King        
The Curious Case of the "Sandia" O1: Oil Hardened Blued Beauty        
The Sword, the Veil, the Legend Elasticity, Stiffness, Stress,
and Strain in Knife Blades
   
Professional Knife Consultant Heat Treating and
Cryogenic Processing of
Knife Blade Steels